Indirect Tensile Strength (ITS) Testing
Overview
Earthbind® Stabilization (EBS) uses Indirect Tensile Strength (ITS) testing as a primary performance-based method for stabilization mix design. ITS testing is used to determine the optimal emulsion content required to stabilize blended aggregates and soils used in base layers.
The objective of ITS-based mix design is to achieve measurable, repeatable performance while meeting or exceeding a minimum ITS strength of 40 psi using the lowest effective emulsion dosage for durability and cost efficiency.
ITS testing is widely recommended by industry organizations, including the Asphalt Recycling and Reclaiming Association (ARRA), for stabilization and recycling mix design.
Why Earthbind Uses ITS
Earthbind® stabilization is intended to create bound base layers, not flexible asphalt surfaces. Performance depends on internal cohesion and binder–aggregate interaction rather than asphalt flow characteristics.
ITS testing directly evaluates this behavior by measuring tensile strength, making it a more meaningful indicator of stabilized base performance than traditional asphalt mix tests.
What Is ITS Testing
Indirect Tensile Strength (ITS) testing measures how well a compacted material resists tensile (pull-apart) forces.
During the test, a cylindrical specimen is loaded across its diameter. The applied load induces tensile stresses within the sample, and the resulting failure reflects the material’s internal cohesion and bonding.
In practical terms, ITS testing answers a critical question: how well does Earthbind®-stabilized material hold together under load?
This makes ITS especially well-suited for evaluating emulsion-stabilized base and soil materials, where performance depends on binder–aggregate bonding rather than asphalt flow.
Why Tensile Strength Matters
Earthbind® stabilization produces bound base materials that depend on cohesion and internal tensile strength and must resist cracking, breakup, and raveling. These materials do not behave like hot-mix asphalt.
Because tensile cracking and cohesion loss are common failure mechanisms in stabilized bases, tensile strength provides a more relevant measure of long-term performance than traditional asphalt-focused tests.
Marshall Testing
Marshall testing was developed for hot-mix asphalt surface courses and was not intended for stabilized base materials.
When applied to Earthbind®-treated bases, Marshall testing focuses on stability and flow rather than cohesion, is designed for high-temperature asphalt mixtures, does not directly measure tensile cracking resistance, and is less sensitive to changes in emulsion content in soil–aggregate blends.
As stabilization practices evolved, ITS testing became the preferred method because it better reflects how stabilized base materials perform in the field.
Why ITS Is Preferred
Earthbind® relies on controlled interaction between binder, aggregates, and soils. ITS testing directly evaluates that interaction.
- Direct measurement of cohesion and tensile strength
- Sensitivity to emulsion dosage changes
- Applicability to soil–aggregate blends
- Correlation with stabilized base performance
- Support from modern industry guidance
For these reasons, ITS testing is used as the primary performance criterion in Earthbind® stabilization mix designs.
Minimum Strength Target
A minimum ITS value of 40 psi is commonly used for stabilized base materials and is widely referenced in industry guidance.
- Demonstrates meaningful improvement over untreated material
- Indicates effective binder–aggregate bonding
- Has a proven record of satisfactory field performance
Earthbind® mix designs typically select the lowest emulsion dosage that consistently meets or exceeds 40 psi to ensure performance without over-treatment.
How ITS Is Used in Mix Design
Earthbind® mix designs follow a structured, performance-based approach.
- Multiple emulsion contents are evaluated, typically ranging from 2% to 4%
- Samples are compacted and cured under controlled conditions
- ITS testing is performed on each mix
- Results are compared to the minimum strength target
The optimal emulsion content is selected based on strength, consistency, constructability, and practical field application.
This approach ensures Earthbind® stabilization is engineered, not guess-based.
Frequently Asked Questions
What does ITS testing tell me as an owner or contractor?
It confirms that the Earthbind®-stabilized material has enough internal strength and cohesion to function as a durable bound base layer.
Why is 40 psi used as the benchmark?
Because it represents a recognized performance threshold that indicates effective stabilization and reliable base performance.
Does a higher ITS value always mean a better mix?
Not always. The goal is to achieve adequate strength with the minimum effective emulsion content. Excess binder can increase cost and may affect constructability.
Why doesn’t Earthbind® use Marshall testing anymore?
Marshall testing was developed for hot-mix asphalt. ITS testing provides a more relevant and reliable measure of performance for emulsion-stabilized bases and soils.
Is ITS testing accepted by the industry?
Yes. ITS testing is widely used by agencies, consultants, and laboratories involved in stabilization and recycling work and is supported by organizations such as ARRA.
Does ITS testing replace all other lab tests?
No. ITS is a key performance test, but it is used alongside gradation, moisture-density relationships, and other material characterization tests as appropriate.
Is there a specific test method used for Indirect Tensile Strength (ITS) testing in Earthbind® mix designs?
Yes. Indirect Tensile Strength (ITS) testing for Earthbind® Stabilization (EBS) mix designs is performed in general accordance with ASTM D6931, Standard Test Method for Indirect Tensile (IDT) Strength of Bituminous Mixtures.
Because ASTM D6931 was originally developed for asphalt mixtures, certain specimen preparation, curing, and conditioning steps are adapted for emulsion-stabilized aggregate and soil materials. These adaptations are standard practice in stabilization mix design and do not affect the validity of the tensile strength measurement.
ITS testing is used by Earthbind® as a mix design and optimization tool, not as construction acceptance testing. A minimum ITS strength of 40 psi is used as the performance benchmark, consistent with common industry guidance.
Summary
Earthbind® uses Indirect Tensile Strength (ITS) testing because it provides a direct, meaningful measure of stabilization performance. This approach ensures that each mix design meets recognized performance targets, uses emulsion efficiently, reflects real-world base behavior, and aligns with modern stabilization practices.
The result is durable, cost-effective, and performance-driven stabilization.
Products
Downloads
- Railway Track Road Stabilization
- Mining Application Protocols: Topical and “Mini Stabilization” Techniques
- Asphalt Emulsion Manufacturing
- TopicalDeep Stabilization Application Protocols
- Earthbind® Safety Data Sheet
- Earthbind® Stabilizer Product Information Packet
- Earthbind® MSDS
- QAS Registration Certificate